A Review on Investigation of Casting Defects with Simulation

Download
Download is available until
  • Version
  • Download 903
  • File Size 0.00 KB
  • File Count 1
  • Create Date 21 July, 2025
  • Last Updated 21 July, 2025

Authors : Akash A. Gaware , Dr. A. K. Mahalle

Abstract: Aim of this paper is to investigate casting defects, provide remedies and simulation of casting process by using casting simulation software. Casting defect occurs where mistake happens in the process of casting. Most defects occur due to improper feeding system. Simulation is helpful in minimizing the casting defects. Various simulation softwares like AutoCAST-X, ProCast & SOLIDCast can be used.